Usage/Application | Industrial |
Surface Finishing | Polished |
Material | Iron |
Design | \ |
Diameter | 25 mm |
Frequency | 50 Hz |
Phase | 1 Ph |
Voltage | 230V |
Brand | METLAB |
Net Weight | Approx 35 Kg |
Overall Dimension | Approx 375 (L) x 285 (B) x 650 (H) mm |
Length | 100 mm |
The most commonly used method for determining hardenability is the end quench test developed by Jominy and Boegehold. The details of the test are covered in ASTM A255
In this test a normalized 25 mm diameter and 100 mm length test sample of steel to be evaluated is heated uniformly to its austenitizing temperature. The specimen is then removed from the furnace and placed in the end quench test Apparatus and immediately end quenched by a jet of room temp. water.
After end quenching, longitudinal Flat Surfaces are ground on opposite sides of the test piece as per dimensions . This grinding is very important for correct positioning of the sample in the fixture and also for accurate repeatable and reliable test results.
MaterialStainless SteelPhaseSingle PhaseDimensions100 +- 0.5mm , dia 25mm +- 0.5 xBrandM... Continue
MaterialMild SteelBrandMetlabVoltage230 VoltsPhaseSingle PhaseLength100 +- 0.5mm... Continue
Voltage230 VoltsMax OperatingTemperature950 or 1150 degree CelsiusFurnace Weight (Kg)50 to 75 kg... Continue